Defects on compressed natural gas (CNG) storage cylinders can often result in damage of costly cylinders. Acoustic emission (AE) testing was performed on type I steel cylinder. These studies suggested ...
Buku sedia untuk dipinjam.
Sila login untuk meminjam buku.
Himeji Works of Godo Steel is a steel plant with EAF, and main product is round bar of carbon steel for structural steel. Recently, quality demands have risen particularly among special steel users. O ...
Buku sedia untuk dipinjam.
Sila login untuk meminjam buku.
Edge cracking is the predominate surface defects in SK85 high carbon steel ([C]=0.85%) that may occur in cold-rolling operation. In this study, the simulation of shearing and rolling of high-carbon st ...
Buku sedia untuk dipinjam.
Sila login untuk meminjam buku.
A stainless steel bar rarely gets rusty and its surface is clean, so it is mainly used for buildings attachments. It is generally peeled and after that sometimes hairline-polished. In this process lus ...
Buku sedia untuk dipinjam.
Sila login untuk meminjam buku.
The injection of pulverized coal has become the most important secondary fuel for blast furnaces once the price for oil and natural gas has started to rise in the 1970s. The purpose is to replace othe ...
Buku sedia untuk dipinjam.
Sila login untuk meminjam buku.